Single phase Ca3Sc2Si3O12 co-doped with Pr3+ and Mg2+ was synthesized by high temperature solid state reaction. The optical spectroscopy of this composition was investigated using time-resolved VUV spectroscopy upon excitation with synchrotron radiation. It was demonstrated that the addition of Mg2+ leads to a significant modification of the luminescence properties in terms of emission intensity, dynamics and reduction of defect concentration in comparison to Mg-free Ca3Sc2Si3O12:Pr3+. The peculiarities of the host-to-impurity energy transfer are analysed and discussed.

VUV Spectroscopy of Ca3Sc2Si3O12:Pr3+: Scintillator Optimization by Co-Doping with Mg2+ Luminescence and Display Materials, Devices, and Processing

PICCINELLI, FABIO;SPEGHINI, Adolfo;BETTINELLI, Marco Giovanni
2012-01-01

Abstract

Single phase Ca3Sc2Si3O12 co-doped with Pr3+ and Mg2+ was synthesized by high temperature solid state reaction. The optical spectroscopy of this composition was investigated using time-resolved VUV spectroscopy upon excitation with synchrotron radiation. It was demonstrated that the addition of Mg2+ leads to a significant modification of the luminescence properties in terms of emission intensity, dynamics and reduction of defect concentration in comparison to Mg-free Ca3Sc2Si3O12:Pr3+. The peculiarities of the host-to-impurity energy transfer are analysed and discussed.
2012
Calcium scandium silicates; Pr3+; VUV spectroscopy; defects; synchrotron radiation; energy transfer
File in questo prodotto:
Non ci sono file associati a questo prodotto.

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/11562/473985
Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus 13
  • ???jsp.display-item.citation.isi??? 11
social impact